Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 5400 min | 90.0 hour | |
3M AC-236 Class B-4 Aerospace Sealant 3M Aerospace Sealant AC-236 Class B are two-component, manganese dioxide cured, liquid polysulfide polymer system providing excellent fuel tank and fuselage seals. They have outstanding resistance t.. |