Polymer Property : Cure Time = 6.50 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Cure Time 1.50 - 6.50 min
0.0250 - 0.108 hour
ts2; ASTM D2084
ExxonMobil Exxon™ 2211 Fast Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is offwhite to amber balesInformation provided by ExxonMobil Chemical
Cure Time 1.50 - 6.50 min
0.0250 - 0.108 hour
ts2; ASTM D2084
ExxonMobil Exxon™ 2222 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product for is white to light amber bales.Information provided by ExxonMobil Chemical
Cure Time 1.50 - 6.50 min
0.0250 - 0.108 hour
ts2; ASTM D2084
ExxonMobil Exxon™ 2235 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene. The product form is white to light amber bales.Information provided by ExxonMobil Chemical
Cure Time 1.50 - 6.50 min
0.0250 - 0.108 hour
ts2; ASTM D2084
ExxonMobil Exxon™ 2255 Regular Cure Rate Grade
Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene.The product form is white to light amber bales.Information provided by ExxonMobil Chemical