Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 7.50 min @Temperature 155 °C |
0.125 hour @Temperature 311 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 7.50 min @Temperature 155 °C |
0.125 hour @Temperature 311 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 7.50 min @Temperature 155 °C |
0.125 hour @Temperature 311 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Cure Time | 7.50 min | 0.125 hour | t`50, Target; ASTM D2084 |
ExxonMobil Exxon™ 2255 Regular Cure Rate Grade Exxon Bromobutyl is a brominated copolymer of isobutylene and isoprene.The product form is white to light amber bales.Information provided by ExxonMobil Chemical |
|||
Cure Time | 7.50 min @Temperature 155 °C |
0.125 hour @Temperature 311 °F |
|
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 2.0 PHR MBTS MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |