Processing Properties Metric English Comments
Cure Time 40.0 - 70.0 min
0.667 - 1.17 hour
Tack-Free, 50% RH
3M 755 Hybrid Sealant
3M™ 700-Series Hybrid Sealant and Hybrid Adhesive Sealant products are one component, moisture curing products which form permanent elastic bonds. They are similar in function as a typical one comp..