Processing Properties Metric English Comments
Cure Time 0.0167 - 43200 min
0.000278 - 720 hour
Average value: 492 min Grade Count:280
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Cure Time 3.00 - 43200 min
0.0500 - 720 hour
Average value: 4860 min Grade Count:57
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Cure Time 10800 - 43200 min
180 - 720 hour
Humiseal 1A27 Urethane Conformal Coating
Humiseal 1A27 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedPasses thermal shock test (MIL-I-46058C)Flammabilit..
Cure Time 10800 - 43200 min
180 - 720 hour
Humiseal 1A27LSE Urethane Conformal Coating
Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C)..
Cure Time 10800 - 43200 min
180 - 720 hour
Humiseal 1A33 Urethane Conformal Coating
Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL..
Cure Time 10800 - 43200 min
180 - 720 hour
Humiseal 1A33LSE Urethane Conformal Coating
Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther..