Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 840 min @Temperature 25.0 °C |
14.0 hour @Temperature 77.0 °F |
Full Cure; Steel |
Loctite® Assure™ 425 Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Cure Time | 840 min | 14.0 hour | |