Recrystallization Temperature 800 - 1010 °C
1470 - 1850 °F
ATI Wah Chang Vanadium
Vanadium is widely dispersed in the earths crust occurring in many types of deposits. Most vanadium is currently obtained as a by-product or co product from titanomagnetites, petroleum, uranium ores..