Recrystallization Temperature 1200 °C
2190 °F
Deformation level - 90%
Plansee MoILQ Molybdenum Incandescent Light Quality
Characteristics:Recrystallization temperature higher than pure MoFiner grain structure than pure MoApplications: This grade was developed for use in the lighting industry. It is more easily formed..
Recrystallization Temperature 1200 °C
2190 °F
Deformation level - 90%
Plansee MW30 Molybdenum-Tungsten
Characteristics:Improved high temperature properties when compared to pure tungstenImproved corrosion resistance compared to pure tungstenEnhanced etchabilityApplications:Manufacture of ZincGlass In..