Processing Properties Metric English Comments
Recrystallization Temperature 1550 °C
2820 °F
Deformation level - 90%
Plansee WL15 Lanthanum Oxide-doped Tungsten
Tungsten alloy suitable for use as ion sources, lamp electrodes and welding electrodes.Characteristics (compared to pure tungsten):Improved creep resistanceHigher recrystallization temperatureMachin..
Recrystallization Temperature 1550 °C
2820 °F
Deformation level - 90%
Plansee MHC Molybdenum-Hafnium-Carbon
Molybdenum is alloyed with hafnium and carbon with extremely fine carbides providing a fine microstructure.Characteristics:Outstanding heat resistanceOutstanding creep resistanceWithstands extreme t..