Processing Properties | Metric | English | Comments |
---|---|---|---|
Roll Temperature | 10.0 - 87.8 °C | 50.0 - 190 °F | |
Entec Hyril® GP355AS Styrene Acrylonitrile Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec |