Roll Temperature 180 - 230 °C
356 - 446 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Roll Temperature 180 - 230 °C
356 - 446 °F
Hotmelt Coating Multi Roller
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..