Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Dew Point = -35.0 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 4060D Sealant Grade PLA
PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6060D Fiber Grade PLA
NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6201D Fiber Grade PLA
NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically ..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6202D Fiber Grade PLA
NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically ..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6204D Fiber Grade PLA
NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically ..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6251D Fiber Grade PLA
NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6302D Fiber Grade PLA
NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6751D Fiber Grade PLA
NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically ..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer
NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6350D Fiber Grade PLA
NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6400D Fiber Grade PLA
NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically ..
Dew Point -35.0 °C
-31.0 °F
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer
Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f..