Polymer Property : Dew Point = 23.0 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Dew Point -40.0 - -5.00 °C
-40.0 - 23.0 °F
Average value: -35.9 °C Grade Count:11
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..