Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 6.0 Month @Temperature 12.8 - 29.4 °C |
6.0 Month @Temperature 55.0 - 85.0 °F |
|
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Shelf Life | 6.0 Month @Temperature 12.8 - 29.4 °C |
6.0 Month @Temperature 55.0 - 85.0 °F |
|
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Shelf Life | 6.0 Month @Temperature 12.8 - 29.4 °C |
6.0 Month @Temperature 55.0 - 85.0 °F |
|
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |