Processing Properties Metric English Comments
Annealing Temperature 760 - 773.9 °C
1400 - 1425 °F
Soft; Cooling: 1 hr/in/max 6hrs; Cool to 1260°F and hold 4 hrs and let furnace cool to 800°F; < 250 HB
Schmolz + Bickenbach Thermodur® 2714 Extra Fine Structure - Hot Work Die Steel
Description: Thermodur 2714 is an Extra Fine Structure (EFS) nickel based tool steel.Characteristics: Excellent high temperature strength; Good toughness; and Good resistance to thermal shockApplica..
Annealing Temperature 760 - 799 °C
1400 - 1470 °F
Soft; Cooling: Furnace 20°F/hour to 1200 °F/ Then air cooled; < 230 HB
Schmolz + Bickenbach Formadur® 2083 Superclean Plastic Mold Steel
Description: Formadur 2083 Superclean is an electro slag remelted (ESR) martensitic stainless steel developed for corrosion resistant applications and Supplied in the annealed conditionCharacteristi..
Annealing Temperature 760 - 800.0 °C
1400 - 1472 °F
Soft; Cooling: Furnace; < 230 HB
Schmolz + Bickenbach Formadur® 2316/2316 ESR Plastic Mold Steel
Increased corrosion resistance in comparison to Formadur 2083, good polishability. Usually this grade is supplied quenched and tempered to 300 HBApplications: Molds for processing plastics with corr..