Annealing Temperature 840 - 900 °C
1540 - 1650 °F
Stress Relief Annealing (min. 0.5 h)
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..
Annealing Temperature 840 - 900 °C
1540 - 1650 °F
Stress Relief Annealing (min. 0.5 h)
Outokumpu 4948 High Temperature Austenitic Stainless Steel
Creep-resistant variant of 1.4301, with a standardized minimum carbon content for service at temperatures of up to 800°C in dry air.Applications: Heat and creep resistance. For use over 550°C for..