Processing Properties | Metric | English | Comments |
---|---|---|---|
Annealing Temperature | 1020 - 1080 °C | 1870 - 1980 °F | Quench Annealing |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Annealing Temperature | 1020 - 1080 °C | 1870 - 1980 °F | Stress Relief Annealing |
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |