Annealing Temperature 399 - 427 °C
750 - 800 °F
Soft; Cooling: Furnace; <230 HB
Schmolz + Bickenbach Thermodur® 2999 Hot Work Die Steel
Description: Maximum high-temperature strength, good high-temperature wear resistance, excellent thermal shock resistance and thermal conductivity across the entire range of service temperatures App..