Processing Properties Metric English Comments
Annealing Temperature 1150 - 1200 °C

@Thickness >=2.00 mm
2100 - 2190 °F

@Thickness >=0.0787 in
Solution Annealing, quench with water
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..