Annealing Temperature 1120 - 1150 °C

@Thickness <=2.00 mm
2050 - 2100 °F

@Thickness <=0.0787 in
Solution Annealing, cooling with air/water
Outokumpu 254 SMO® High Performance Austenitic Stainless Steel
Applications: Process equipment in chemical industryBleaching equipment in the pulp and paper industryFlue-gas cleaningDesalinationSeawater handlingHeat exchangersAvailable in hot rolled plate (Quar..