Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Gel Time 0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
hot plate
3M Scotchcast™ 260 Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to..
Gel Time 0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
hot plate
3M Scotchcast™ 262 Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 262 is a widely used, well-known general purpose epoxy powder resin. A one-part, red pigmented, rapid heat-curing product, it is designed to provide a continuous, toug..
Gel Time 0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 193 °C
0.200 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 379 °F
hot plate
3M Scotchcast™ 260 CG Electrical Epoxy Powder Resin
3M Scotchcast Electrical Resin 260 is a widely used, well-known general purpose epoxy powder resin. A one-part, green pigmented, rapid heat-curing product, it is designed to provide a continuous, to..