Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 1380 min | 1380 min | |
ACC QLE 1035 QSI Quantum Silicones 38 Durometer Addition Cure Elastomer for Coating QLE 1035 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |