Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 8.00 - 14.0 min | 8.00 - 14.0 min | |
Master Bond EP65HT Fast Setting Epoxy Resists High Temperatures Description: Master Bond EP65HT represents a highly innovative advance in epoxy technology in that it features the unusual combination of very fast cures and high temperature resistance. While typic.. |
|||
Gel Time | 12.0 - 14.0 min @Temperature 120 °C |
12.0 - 14.0 min @Temperature 248 °F |
|
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix HexPly® M49 is a 120°C curing toughened epoxy matrix with good impact resistance suitable for use in performance cars. The matrix is highly tolerant of a wide variety of production techniques and .. |