Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 17.0 min | 17.0 min | 3M Method TM-67 |
3M Scotchcast™ 2130 Flame-Retardant Compound 3M Scotchcast Flame-Retardant Compound 2130 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. Its unique formulation makes it.. |
|||
Gel Time | 17.0 min | 17.0 min | 3M Method TM-87 |
3M Scotchcast™ 2131 Flame-Retardant Compound 3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particu.. |