Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 1.00 - 2.50 min | 1.00 - 2.50 min | |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Gel Time | 0.800 - 2.50 min @Temperature 135 °C |
0.800 - 2.50 min @Temperature 275 °F |
|
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |
|||
Gel Time | 0.800 - 2.50 min @Temperature 135 °C |
0.800 - 2.50 min @Temperature 275 °F |
|
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |