Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 120 - 240 min @Temperature 25.0 °C |
120 - 240 min @Temperature 77.0 °F |
Thin Film |
Trelleborg Emerson & Cuming EP574 Adhesive Clear unfilled adhesive for thin bond lines.All information provided by Trelleborg Emerson & Cuming |