Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 30.0 - 60.0 min | 30.0 - 60.0 min | |
Resin Technology Group FDA-24N Two component Polyurethane Adhesive Resin Technology Group FDA-24N Two component Polyurethane AdhesiveFDA approvable, 1:1 ratio, general purpose adhesive |
|||
Gel Time | 30.0 min | 30.0 min | Slow |
ACC EP RASP EPI Engineered Polymers Aliphatic Silicone Polymer EP RASP Aliphatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea that has excellent UV stability (colorfast) with superior performance in industria.. |
|||
Gel Time | 30.0 min | 30.0 min | 75°C |
ACC EP RAP 60 EPI Engineered Polymers Aliphatic Polyurea EP RAP 60 Aliphatic Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solids, no VOC, coating (silicone optional) developed for UV stable (colorfast) polyurea flooring applic.. |