Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 5.50 min @Temperature 120 °C |
5.50 min @Temperature 248 °F |
|
Hexcel® HexPly® M27 248°F (120°C) Curing Epoxy Matrix HexPly® M27 is specifically designed for applications with fast curing cycles. It is ideally suited for high volume production techniques-in particular for ski manufacture. HexPly® M27 has been sp.. |