Processing Properties | Metric | English | Comments |
---|---|---|---|
Gel Time | 2.00 - 8.00 min | 2.00 - 8.00 min | |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Gel Time | 2.00 - 8.00 min | 2.00 - 8.00 min | |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, G30-700 Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Gel Time | 2.00 - 8.00 min | 2.00 - 8.00 min | |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Gel Time | 5.00 - 8.00 min @Temperature 177 °C |
5.00 - 8.00 min @Temperature 351 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin HexPly® F650 is a bismaleimide resin that cures via an additional/free radical mechanism resulting in a cross-linked thermoset system with no condensation by-products. HexPly® F650 was developed b.. |