Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 300 - 420 min @Temperature 60.0 °C |
300 - 420 min @Temperature 140 °F |
|
Abatron AboCast/AboCure 8109-5 High heat resistance. Easy to use.Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure.Applications.. |
|||
Pot Life | 45.0 - 420 min @Temperature 60.0 °C |
45.0 - 420 min @Temperature 140 °F |
|
Abatron AboCast/AboCure 8109-7 Processing: 100/80 pbw; Potlife: 6-7 days/20°C (68°F), 12-24 h/40°C (105°F), 0.75-7 h /60°C (140°F); mix at 50-80°C (120-175°F); cures in: 1 h/100°C (212°F) + 4 h/150°C (300°F) postcure... |