Polymer Property : Pot Life = 540 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 420 - 540 min

@Temperature 23.9 °C
420 - 540 min

@Temperature 75.0 °F
100 g batch
Master Bond Super Gel 9 Two component urethane modified epoxy gel-like system
Cures at room temperature to form a soft, resilient gel-like system with good dimensional stability. It has excellent optical clarity, convenient to handle, and is easy to retrieve with a sharp kni..