Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 191 - 204 °C | 376 - 399 °F | |
PolyOne Geon™ Vinyl Rigid Extrusion 87560 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Melt Temperature | 191 - 199 °C | 376 - 390 °F | |
PolyOne Geon™ Vinyl Dry Blend E6001 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 191 - 204 °C | 376 - 399 °F | |
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid) Interior application for thick & thin gauge profile application.Information provided by PolyOne |
|||
Melt Temperature | 191 - 204 °C | 376 - 399 °F | |
PolyOne Geon™ Vinyl Dry Blend E6950 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Melt Temperature | 191 - 196 °C | 376 - 385 °F | |
PolyOne Geon™ Vinyl Flexible B8503 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne |
|||
Melt Temperature | 191 - 202 °C | 376 - 396 °F | |
PolyOne Geon™ Vinyl Flexible B87FB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 191 - 196 °C | 376 - 385 °F | |
PolyOne Geon™ Vinyl Flexible FC801 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 191 - 196 °C | 376 - 385 °F | |
PolyOne Geon™ Vinyl Flexible FC900 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 191 - 229 °C | 376 - 444 °F | Injection |
Samsung Cheil Industries Starex® SD-0150 ABS, Unreinforced
(discontinued **) Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: General Purpose: Good Impact Strength, Chemical Resistance, ProcessabilityApplications: Household Appliances, Auto Interior Trim and P.. |
|||
Melt Temperature | 191 - 202 °C | 376 - 396 °F | |
PolyOne Geon™ Vinyl Flexible 86479 Opaque Polyvinyl Chloride Information provided by PolyOne |
|||
Melt Temperature | 191 - 202 °C | 376 - 396 °F | |
PolyOne Geon™ Vinyl Flexible 86479 Tran Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 191 - 202 °C | 376 - 396 °F | |
PolyOne Geon™ Vinyl Flexible B80MB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 191 - 196 °C | 376 - 385 °F | |
PolyOne Geon™ Vinyl Flexible B8502 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible PVC Compound with good resistance to migration to specific applications.Information provided by PolyOne |
|||
Melt Temperature | 191 - 196 °C | 376 - 385 °F | |
PolyOne Geon™ Vinyl Flexible FC800 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 191 - 202 °C | 376 - 396 °F | |
PolyOne Geon™ Vinyl Flexible R267AM Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 191 - 210 °C | 376 - 410 °F | Average value: 203 °C Grade Count:11 |
Overview of materials for Chlorinated PVC (CPVC) This property data is a summary of similar materials in the MatWeb database for the category "Chlorinated PVC (CPVC)". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melt Temperature | 191 °C | 376 °F | |
DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se.. |
|||
Melt Temperature | 191 °C | 376 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 191 °C | 376 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 191 °C | 376 °F | |
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:.. |
|||
Melt Temperature | 191 °C | 376 °F | |
DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Melt Temperature | 191 °C | 376 °F | |
DuPont™ Surlyn® 1901 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1901 is a sodium ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultr.. |
|||
Melt Temperature | 191 - 202 °C | 376 - 396 °F | |
PolyOne Geon™ CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC) Geon LC500 CPVC is an extrusion grade rigid compound. It is designed for applications where enhanced resistance at elevated temperatures is needed. LC500 demonstrates ease of processing with excelle.. |
|||
Melt Temperature | 191 - 196 °C | 376 - 385 °F | |
PolyOne Geon™ Vinyl Wire & Cable W1202 Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 191 °C | 376 °F | |
DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry,.. |
|||
Melt Temperature | 191 °C | 376 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Melt Temperature | 191 °C | 376 °F | Injection |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 22% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |