Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 154 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 143 - 154 °C
289 - 309 °F
Huntsman PE1058 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability, excellent strength, good heat sealability, and optics.Applications: Film extrusion: all thin film uses and especiall..
Melt Temperature 143 - 154 °C
289 - 309 °F
Huntsman PE1068 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional draw down and processability even to 1/2 mil; excellent strength, good heat sealability, and good optical.FDA Notes: Conforms to FDA regulation 21..
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.
Melt Temperature 143 - 154 °C
290 - 310 °F
A. Schulman SCHULAMID® 66 GF50 50% Glass Fiber Reinforced 66
Information provided by A. Schulman.