Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 145 - 155 °C | 293 - 311 °F | |
EMS-Griltech Grilene® KE 150 CoPES Mono-Component Fusible Adhesive Fiber Description: Grilene KE 150 is the well known CoPES mono-component fusible adhesive fiber. It is used in compact dry-laid nonwoven.Data provided by EMS-Griltech. |