Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJJX206L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B65F1 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 171 °C | 334 - 340 °F | |
PolyOne Geon™ Vinyl Wire & Cable WJAF111L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Melt Temperature | 168 - 274 °C | 335 - 525 °F | Average value: 221 °C Grade Count:17 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Temperature | 168 - 174 °C | 334 - 345 °F | |
PolyOne Geon™ Vinyl Flexible C6502 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 177 °C | 334 - 351 °F | |
PolyOne Geon™ Vinyl Flexible C70A0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8600-85 Clear PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8925-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8950-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8960-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8980-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 8999-85 Natural PVC Extrusion Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9077-85 LMW Natural PVC for Injection Molding Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9915-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9925-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9940-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9950-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 - 179 °C | 335 - 355 °F | |
Sylvin Technologies 9980-85 Natural PVC Molding Compound Information provided by Sylvin Technologies Inc. |
|||
Melt Temperature | 168 °C | 335 °F | Processing Temperature |
Teknor Apex APEX® 1008 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3201-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMUses-Automotive Applications, Non-specific Food Applications, General Purpose, Medical Applications, Modeling.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3300-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Food Service Applications, General Purpose, Me.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3311-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3200-60 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 11600 Wire & Cable Flexible PVC Clear, non-staining speaker wire insulation and general purpose extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 8552 Moldings & Extrusions Flexible PVC A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 8758 Moldings & Extrusions Flexible PVC A general purpose extrusion compound recommended for extruded shapes, weatherstrips and flexible gaskets. Formulated for good UV light resistance and low temperature properties.Information provided.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 10703 Wire & Cable Flexible PVC Non-lead stabilized general purpose jacketing compound with good low temperature properties. Recommended for a maximum service temperature of 80°C at a 15 mil wall thickness.Information provided b.. |
|||
Melt Temperature | 168 °C | 335 °F | |
Teknor Apex APEX® 3311-60NT Polyvinyl Chloride, Flexible Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications; Toys; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Temperature | 168 °C | 335 °F | |
Axiall 22750 Coax & Telecom Flexible PVC Non-staining extrusion compound recommended for retractile telecommunication cord. Maximum service temperature of 60°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |