Polymer Property : Melt Temperature = 208 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 208 °C
406 °F
Honeywell Aegis™ OX High Barrier Nylon  (discontinued **)
Description: Aegis OX is an oxygen-scavenging nylon. Oxygen barrier is comparable to a glass bottle with metal crown closure. In addition Aegis OX provides CO2 barrier and possesses glass-like cla..