Processing Properties Metric English Comments
Melt Temperature 1200 - 1280 °C
2190 - 2330 °F
Wieland Euro 50 PFM Alloy
Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental