Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Melt Temperature | 216 - 241 °C | 421 - 466 °F | |
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi.. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 111-35 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Melt Temperature | 193 - 241 °C | 380 - 465 °F | Processing |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |