Processing Properties Metric English Comments
Melt Temperature 125 - 130 °C
257 - 266 °F
Polyplastic Torlen® PE 2K 901 High Density Polyethylene, Carbon Filled
Information provided by PolyPlastic Group.
Melt Temperature 125 - 130 °C
257 - 266 °F
Borealis Supercure™ LC8205R Polyethylene Insulation Compound, Crosslinkable
Supercure™ LC8205R is a crosslinkable natural polyethylene compound, specially designed for insulation applications. Applications: Supercure™ LC8205R is intended for insulation of XLPE power cabl..