Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 147 °C | 297 °F | ASTM D4591 |
Westlake Plastics Propylux® Void-Free Polypropylene Propylux is made from polypropylene resin. Among its most notable characteristics are its mechanical toughness, chemical resistance and resistance to abrasion. These properties make it suitable fo.. |