Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 349 - 377 °C | 660 - 711 °F | injection molding |
Solvay Specialty Polymers Radel® R-7120 Polyphenylsulfone, 20% glass fiber
(discontinued **) RADEL R 7120 is a 20% glass fiber reinforced grade of RADEL R polyphenylsulfone developed specifically for aircraft interior applications. The product complies with the FAA regulation 14CFR Part 25 .. |
|||
Melt Temperature | 354 - 377 °C | 670 - 710 °F | Molding |
PolyOne Edgetek® PF-40CF/000 Polysulfone, Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Melt Temperature | 343 - 377 °C | 649 - 711 °F | Stock |
PolyOne Stat-Tech™ RA-06CF-09GF/000 Polyarylsulfone - 9% Glass Fiber - 6% Carbon Fiber Reinforced - ESD Applications
&a Data provided by PolyOne. |
|||
Melt Temperature | 343 - 377 °C | 649 - 711 °F | Stock |
PolyOne Stat-Tech™ RA-06CF-09GF/000 EM Polyarylsulfone - ESD Applications - Flow Enhanced Grade
(discontinued Data provided by PolyOne. |