Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 228 °C | 442 °F | |
E-Polymers SEPAZ® N5030 Nanoclay 4%, 30% Glass Fiber Reinforced Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Melt Temperature | 228 °C | 442 °F | |
E-Polymers SEPAZ® N6030FR 30% Glass Fiber Reinforced Flame Retardant Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |
|||
Melt Temperature | 228 °C | 442 °F | |
E-Polymers SEPAZ® N6000FR Nanoclay 4% Flame Retardant Nano Composite Resin Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi.. |