Polymer Property : Melt Temperature = 80.6 °C
Polymer Property :
Melt Temperature =
80.6 °C
Product List
Processing Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties
Metric
English
Comments
Melt Temperature
80.6
-
83.3
°C
177
-
182
°F
PolyOne Geon™ Vinyl Flexible A90F1 Polyvinyl Chloride, Flexible (PVC, Flexible)
Recommended for interior applications.Information provided by PolyOne