Electrical Properties Metric English Comments
High Voltage Arc Resistance to Ignition (HVAR) 60 - 120 sec

@Thickness 3.00 mm
60 - 120 sec

@Thickness 0.118 in
UL 746A
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM
Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva..