Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000203 ohm-cm | 0.00000203 ohm-cm | Bar, Rod & Forgings (85 % IACS) |
CMW® 3 Copper Alloy CMW® 3 material is a high strength, high conductivity copper base alloy. CMW® 3 material is heat treatable. Optimum mechanical and physical properties of CMW® 3 material are developed by heat tre.. |
|||
Electrical Resistivity | 0.00000203 ohm-cm | 0.00000203 ohm-cm | 85 % IACS |
CMW® DSC Copper with Dispersed Aluminum Oxide CMW® DSC material is an extruded and cold worked powder metallurgy material consisting of copper and dispersed aluminum oxide. It has exceptional high temperature strength for its electrical conduc.. |