Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000180 - 0.00000210 ohm-cm | 0.00000180 - 0.00000210 ohm-cm | |
Williams Advanced Alloys C118 Solder Williams extensive offering of Contact Alloys are cast and fabricated to meet the exacting standards of various micro electronics applications. All Williams electrical contact alloys are available i.. |