Electrical Properties Metric English Comments
Electrical Resistivity 0.00000339 ohm-cm

@Diameter 0.762 mm
0.00000339 ohm-cm

@Diameter 0.0300 in
annealed wire with 0.22% Li
Lucas-Milhaupt Lithobraze 720 (BT) Silver Based Cadmium Free Filler Metal
Applications: Litho braze 720 is a good general purpose, low temperature filler metal of high fluidity for fluxless furnace brazing of stainless steels when used in dry hydrogen or inert atmosphere..