Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000344 - 0.00000382 ohm-cm | 0.00000344 - 0.00000382 ohm-cm | Conductivity is 45-50% IACS |
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Electrical Resistivity | 0.00000344 - 0.00000382 ohm-cm | 0.00000344 - 0.00000382 ohm-cm | Conductivity is 45-50% IACS |
Materion BrushCAST® 3C High Conductivity Casting Alloy (As Cast) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |
|||
Electrical Resistivity | 0.00000344 - 0.00000382 ohm-cm | 0.00000344 - 0.00000382 ohm-cm | Conductivity is 45-50% IACS |
Materion BrushCAST® 3C High Conductivity Casting Alloy (Solution Annealed & Aged) Pouring Temperature: 1095-1175°CHeat treatment required for max strength (Annealing): 870-900°C/water quenchHeat treatment required for max strength (Hardening): 870-900°C/water quenchDescr.. |