Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000344 - 0.00000410 ohm-cm | 0.00000344 - 0.00000410 ohm-cm | Calculated from 42-50 %IACS |
Cadi 10WC Tungsten Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |
|||
Electrical Resistivity | 0.00000344 - 0.00000410 ohm-cm | 0.00000344 - 0.00000410 ohm-cm | Calculated from 42-50 %IACS |
Cadi 5TC Tungsten Carbide Copper Available in a variety of rounds, rectangles, and shapes.Information provided by Cadi Company. |