Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | |
Hogen Duralloy H10TC 56 Tungsten Carbide/44 Copper PM Metal Composite Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for heavy-duty or projection w.. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | |
Mi-Tech Metals TC56 56 Tungsten Carbide/44 Copper PM Metal Composite Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for heavy-duty or projection welding .. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | precipitation hardened (2 hr) |
CLAL-MSX SICLANIC S® TB Quenched Copper Alloy SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | precipitation hardened (3 hr) |
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | precipitation hardened (4 hr) |
CLAL-MSX SICLANIC S® TD4 Quenched Copper Alloy, 4/4 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | precipitation hardened (5 hr) |
CLAL-MSX SICLANIC S® TH3 Quenched Copper Alloy, 1/2 Hard, precipitation treated SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | precipitation hardened (2 hr) |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | precipitation hardened (3 hr) |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |
|||
Electrical Resistivity | 0.00000420 ohm-cm | 0.00000420 ohm-cm | precipitation hardened (4 hr) |
CLAL-MSX SICLANIC S® TD3 Quenched Copper Alloy, 1/2 Hard SICLANIC S® is particularly recommended for the production of conductive contact blades. SICLANIC S® offers :electrical conductivity greatly superior to that of bronzes, brasses and nickel silver.. |